https://www.avient.com/sites/default/files/resources/TPE_Overmolding_Solutions_for_Engineering_Thermoplastics.pdf
Materials Temperature, C, Nozzle/Front/Middle/Rear Mold Temperature, C Injection Hi Pressure, psi OM1040 430/430/410/390 80 500 OM1060 430/430/410/390 80 600 OM1245 430/430/410/390 80 500 OM1262 430/430/410/390 80 800 OM6050 480/480/460/440 80 1000 OM6065 480/480/460/440 80 1200 B-TPE-35A 450/450/430/410 80 500 B-TPE-50A 450/450/430/410 80 800 B-TPE-65A 450/440/430/420 80 800 B.TPV-55A 480/480/470/460 80 800 B-TPV-55A 525/520/510/490 110 1500 B-TPV-70A 535/530/520/500/ 110 1500 Table 5: Typical Flow lengths achievable with GLS compounds.
Injection velocity, 5 in/s OM-1040 360 OM-1060 417 OM-1255 246 OM-1262 379 OM-6050-9 253 OM-6065-9 221 60A S-TPE 329 64A TPV 228 Table 5: Materials Temperature, C, Nozzle/Front/Middle/Rear Mold Temperature, C Injection Hi Pressure, psi OM1040 430/430/410/390 80 500 OM1060 430/430/410/390 80 600 OM1245 430/430/410/390 80 500 OM1262 430/430/410/390 80 800 OM6050 480/480/460/440 80 1000 OM6065 480/480/460/440 80 1200 B-TPE-35A 450/450/430/410 80 500 B-TPE-50A 450/450/430/410 80 800 B-TPE-65A 450/440/430/420 80 800 B.TPV-55A 480/480/470/460 80 800 B-TPV-55A 525/520/510/490 110 1500 B-TPV-70A 535/530/520/500/ 110 1500 Figure 2: Effect of overmold thickness on surface hardness on TPE products. 0.0 10.0 20.0 30.0 40.0 50.0 60.0 70.0 80.0 90.0 100.0 0 2 4 6 8 10 Thickness, mm H ar dn es s, S ho re A 12 CL2000X G6713 G7930 G7960 G7980 Adhesion Testing and Results Design Considerations Conclusions
https://www.avient.com/sites/default/files/2022-06/Maxxam FR Injection Molding Processing Guide.pdf
Barrel Temperatures °F (°C) PP Mineral-Filled PP Glass-Filled PP HDPE LDPE Rear Zone 360–390 (182–200) 400–420 (204–216) 415–435 (213–224) 400–420 (204–216) 370–390 (188–199) Center Zone 370–400 (188–204) 410–430 (210–221) 425–445 (218–229) 410–430 (210–221) 380–400 (193–204) Front Zone 390–410 (200–210) 420–440 (216–227) 435–455 (224–235) 420–440 (216–227) 390–410 (199–210) Nozzle 400–425 (204–219) 415–435 (213–224) 430–450 (221–232) 430–450 (221–232) 400–425 (204–219) Melt Temperature 400–425 (204–219) 415–435 (213–224) 430–450 (221–232) 430–450 (221–232) 400 - 425 (204–219) Mold Temperature °F (°C) 60–120 (16–49) Pack & Hold Pressure 50–75% of injection pressure Injection Velocity (in/s) 1.0–3.0 Back Pressure (psi) 50–100 Screw Speed (rpm) 30–100 Drying Parameters Hours @ °F (°C) Not typically required.