https://www.avient.com/sites/default/files/2023-01/CFA Product Selection Guide.pdf
Product Name Material/ Product Code Type Initiation Temp, C Optimum Gas Yield Temp, C Gas Yield Range, cc/g Uses/ Applications Usage Resins POWDER Hydrocerol BIH PEAUFF Endo 140 160 140–150 • Weight reduction • Sink mark removal • Warpage reduction EVA, polyethylene, PE copolymers, TPEs/TPOs, PVC Hydrocerol Compound EMASAD Endo 140 200 135–145 • Weight reduction • Sink mark removal • Warpage reduction Polyethylene, polypropylene, TPEs/TPOs, styrenes, acrylics, TPUs, POM, PVC Hydrocerol HK EMA0766025 Endo 200 210 135–145 • Weight reduction • Sink mark removal • Warpage reduction Polypropylene, styrenes, acrylics, polyamides Hydrocerol 1480 EMA0766027 Endo-Exo 140 180 240–259 • Weight reduction • Sink mark removal • Warpage reduction EVA, polyethylenes, PE copolymers, TPEs/TPOs, styrenes, acrylics, PVC Product Name Material/ Product Code Type Initiation Temp, C Optimum Gas Yield Temp, C Gas Yield Range, cc/g Uses/ Applications Usage Resins MASTERBATCH Hydrocerol 862 PLASAD Endo 140 160 10–20 • Sink mark removal • Warpage reduction EVA, polyethylene, PE compolymers, TPOs/TPEs Hydrocerol BIH-40-E PLASAF Endo 140 160 55–65 • Weight reduction • Sink mark removal • Warpage reduction EVA, polyethylene, PE compolymers, TPOs/TPEs Hydrocerol 1004 PEAUFQ Endo 140 160 80–90 • Weight reduction EVA, polyethylene, PE compolymers, TPOs/TPEs Hydrocerol CF-5-E PEASCF Endo 140 200 5–10 • Sink mark removal • Warpage reduction Polyethylene, polypropylene, TPEs/TPOs, styrenes, acrylics, TPUs, POM Hydrocerol 1602 PRASAD Endo 140 200 50–60 • Weight reduction • Sink mark removal • Warpage reduction Polyethylene, polypropylene, TPEs/TPOs, styrenes, acrylics, TPUs, POM Hydrocerol PEA0820021 PEA0820021 Endo 140 200 25–35 • Weight reduction • Sink mark removal • Warpage reduction Styrenes Hydrocerol PEA08200095 PEA0820095 Endo-Exo 140 180 100–120 • Weight reduction • Sink mark removal • Warpage reduction PVC Hydrocerol ITP-820 PRAN698588 Endo 200 210 5–10 • Sink mark removal • Warpage reduction EVA, polyethylene, PE copolymers, TPEs/TPOs, PVC Hydrocerol HK-40-E PLASAH Endo 200 210 55–65 • Weight reduction • Sink mark removal • Warpage reduction Polyethylene, polypropylene, TPEs/TPOs, styrenes, acrylics, TPUs, POM, PVC Hydrocerol CT-3205-B OMA0698633 Endo 200 210 50–60 • Weight reduction • Sink mark removal • Warpage reduction PLA Hydrocerol 1135 PEAN698616 Exo 170 190 20–30 • Sink mark removal • Warpage reduction Polyethylene, polypropylene, TPEs/TPOs, styrenes, acrylics, TPUs, POM Hydrocerol 8418M PHA0698418 Exo 170 190 50–60 • Weight reduction • Sink mark removal • Warpage reduction Polyethylene, polypropylene, TPEs/TPOs, styrenes, acrylics, TPUs, POM Product Name Material/ Product Code Type Initiation Temp, C Optimum Gas Yield Temp, C Gas Yield Range, cc/g Uses/ Applications Usage Resins MASTERBATCH Hydrocerol 141 PEASCH Exo 200 210 10–20 • Sink mark removal • Warpage reduction Polypropylene, styrenes, acrylics, polyamides Hydrocerol 1191 PRAN698433 Exo 200 210 55–65 • Weight reduction • Sink mark removal • Warpage reduction Polypropylene, styrenes, acrylics, polyamides Hydrocerol NBA0820012 NBA0820012 Exo 240 260 25–35 • Weight reduction • Sink mark removal • Warpage reduction Polyesters, high-temperature resins Hydrocerol XH-901 SAASCC Exo 240 260 30–40 • Weight reduction • Sink mark removal • Warpage reduction Polycarbonate blends, polycarbonate, high-temperature resins Hydrocerol 1376-4 PRAN698541 Endo-Exo 200 210 90–100 • Weight reduction • Sink mark removal • Warpage reduction Polypropylene, styrenes, acrylics, polyamides, PVC LIQUID Excelite FA-37 CC10212522 Endo-Exo 120 140 65–75 • Weight reduction/ WPC Polyethylene Excelite PF-1 CC01053625 Endo-Exo 120 140 55–65 • Weight reduction Vinyl Excelite FA-185 CC10303252 Endo 140 200 75–85 • Weight reduction • Direct gas assist Polyolefin Excelite Foam PPRO CC10250288 Endo 160 200 50–60 • Weight reduction • Warpage reduction Polypropylene Excelite FA-77 CC10232527 Endo-Exo 120 140 85–95 • Weight reduction/ WPC Polyethylene Excelite FA-108 CC10290626 Endo 180 200 55–65 • Weight reduction • Sink mark removal Polyolefin Excelite FA-112 CC10313065 Endo 140 200 50-60 • Weight reduction • Sink mark removal Polyolefin 1.844.4AVIENT www.avient.com Copyright © 2022, Avient Corporation.
https://www.avient.com/sites/default/files/2020-10/tpes-for-automotive-fasteners-clips-product-bulletin-1.pdf
GLS™ TPE AUTOMOTIVE SOLUTIONS ENABLE LONG-TERM PERFORMANCE WITH TPEs FOR FASTENERS AND CLIPS The average length of vehicle ownership is on the rise, placing greater demands on all elastomeric materials to maintain long-term sealing performance in fasteners and clips.
OnFlex™ TPEs provide a tight seal over these lengthier time frames—even at elevated temperatures—and reduce vibration and noise.
ONFLEX™ HT ONFLEX™ AF 7210 ONFLEX™ S KA ONFLEX™ S KG Applications Fasteners/ Clips Fasteners/ Clips Fasteners/ Clips Fasteners/ Clips Defining Characteristic High temperature sealing performance Ambient temperature sealing performance High temperature sealing performance Ambient temperature sealing performance Density 1.00 g/ml 0.99 g/ml 1.10 g/ml 1.13 g/ml Physical Properties Tensile Strength 6.0–10.0 MPa 5.0–11.5 MPa 3.0–7.5 MPa 2.6–4.9 MPa Tear Resistance 25.0–37.0 kN/m 21.0–43.0 kN/m 17.0–46.0 kN/m 16.0–29.0 kN/m Compression Set 73°F (23°C) 72hrs 12–27% 16–32% 13–23% 31–35% 158°F (70°C) 22hrs 28–44% 32–43% 29–38% 62–66% 212°F (100°C) 22hrs 45–53% 56–60% 54–57% 80–85% Hardness 40–80 Shore A 40–80 Shore A 40–80 Shore A 40–80 Shore A Overmolding Substrate Polypropylene/ Polyethylene Polypropylene Polyamide Polyamide Processing Injection Molding/ Extrusion Injection Molding/ Extrusion Injection Molding/ Extrusion Injection Molding/ Extrusion HOW GLS TPEs MAKE THE DIFFERENCE IN AUTOMOTIVE FASTENERS AND CLIPS • Low compression set – coupled with good stress relaxation, our automotive TPEs are designed to maintain a good seal over time and reduce noise generated by vibration • High temperature performance – Avient automotive TPEs provide good sealing performance in temperatures up to 100°C/212°F • Bonding performance - strong chemical bond to polypropylene, polyethylene, and polyamide • Process flexibility - grades can be both injection molded and extruded • Easy to color - can be colored at the machine • Reduced production steps - some grades do not require pre-drying • Low VOC/FOG - OnFlex HT™ has been externally tested to VDA 278 and is proven to help satisfy vehicle interior air quality (VIAQ) regulatory requirements • Single source supply – we can streamline your supply chain with the ability to provide polymer colorants, engineered thermoplastics, and thermoplastic elastomers from a single source • Global support - we provide production, technical, and commercial support in locations convenient to your operations, including North America, Europe, and Asia To learn more about GLS TPEs for automotive applications, visit www.avient.com or call +1.844.4AVIENT (1.844.428.4368). www.avient.com Copyright © 2020, Avient Corporation.