https://www.avient.com/sites/default/files/2023-06/Omnicolor Brochure.pdf
Care
should be used when processing
Omnicolor where melt temperatures
may exceed 600°F (316°C).
For
polymer drying in excess of 225°F
(107°C), add the colorant after the
drying process, or alternatively
contact Avient’s technical staff for
availability of high-temperature
grades.
Calculate using Let Down Percentage:
Cost/lb of Concentrate x (Let Down Percentage/100) = Coloring Cost
Calculate using Let Down Ratio:
Cost/lb of Concentrate – Cost/lb of Resin
Let Down Ratio +1
= Coloring Cost
TWO WAYS TO CALCULATE COLORING COSTS
OMNICOLOR™
TROUBLESHOOTING
TWO WAYS TO CALCULATE COLORING COSTS
SYMPTOM CAUSE REMEDY
Color Variation Shot-to-Shot
Poor Omnicolor preblending
Pigment has insufficient
thermal stability
More thorough blending
Ensure correct machine
temperature control
Screw Slip
Premature melting of Omnicolor
Excessive addition rate
Reduce heat in feed zone
Check addition rate and reduce
if necessary
Overall Good Distributive
Mixing With Streaks or Dots
of Another Color
Poor pigment dispersion in
concentrate
Return concentrate for
replacement
Black Streaks or Splotches Degraded polymer in barrel Clean screw and barrel
Poor Distributive Mixing
(Streaking)
Insufficient plastification See processing instructions
Loss of Color
Pigment has insufficient
thermal stability
Change to more heat stable
colorant
Ensure correct machine
temperature control
OMNICOLOR™
PROCESSING TEMPERATURES
RECOMMENDED MAXIMUM PROCESSING TEMPERATURES FOR OMNICOLOR IN SELECTED POLYMERS IN °C
UK
COLOR NO.
https://www.avient.com/sites/default/files/2022-11/Seat Buckle System Application Snapshot.pdf
TIER 1 SUPPLIER
S E A T B U C K L E S Y S T E M
• Rapid development of 3 colors for global OEM platform, for
3 materials (POM, SAN, PP)
• Help Tier 1 transition from printing to laser marking of
buckles
• Develop formulation that offers laser marking solution plus
color
• Quick reaction to develop three colors for
this global vehicle launch
• Smartbatch™ color + laser marking
formulation met requirements for critical
safety components
Smartbatch™ Combination Colorants &
Additives
KEY REQUIREMENTS
WHY AVIENT?
https://www.avient.com/sites/default/files/2020-12/case-study-versaflex-ce-antimicrobial-phone-case-1.pdf
PHONE CASE
BRAND
P H O N E C A S E S
• Compatible with antimicrobial additives
• Good stain resistance
• Non-yellowing
• Delivered enhanced solution that included
antimicrobial properties and stain resistance
• Collaborated with OEM and the foremost
supplier of antimicrobials to comply with key
bacterial growth requirements
Versaflex™ CE 3320-80 TPE
KEY REQUIREMENTS
WHY AVIENT?
https://www.avient.com/sites/default/files/2024-06/Avient Melle - 2024.pdf
Bergmann GmbH
Adolf-Dambach-Str. 2-4
76571 Gaggenau
c/o Avient ECCOH High Performance Solutions GmbH
Oldendorfer Straße 9, 49324 Melle
Produktion von technischen Thermoplasten
https://www.avient.com/sites/default/files/2024-05/CCG Application Snapshot_PTFE Wire Insulation.pdf
PTFE Wire insulation
W I R E & C A B L E O E M
P T F E W I R E I N S U L A T I O N
• Avoid contamination risks resulting from dry pigments
• Powder paste extrusion process
• High quality dispersion
• Availability of custom color options
• Optimized pigment particle size and distribution to
achieve high-quality dispersion
• Provided a technology based on high-quality
pigments and ready-to-use formulations
• Offered a liquid pigment portfolio as standard in a
wide range of shades with color-matching
capabilities
• Improved the stability and efficiency of the
manufacturing process
Colorant Chromatics PTFE Dispersed
Pigment Solutions
KEY REQUIREMENTS
WHY AVIENT?
https://www.avient.com/sites/default/files/2024-03/LubriOne PKE - Storage Box Latch case study snapshot.pdf
AU TO M OT I V E
A F T E R M A R K E T
M A N U FAC T U R E R
S T O R A G E B O X L A T C H
• Low coefficient of friction (CoF) to allow for ease-of-use
• Colorable to a brand-specified Pantone color
• Low odor in the end product
• Maintain performance when exposed to outdoor elements
and extreme temperatures
• Offered lubricious polyketone (PK) material to
facilitate easy slide and effective latching
• Provided excellent chemical resistance to
cleaning and harsh chemicals, such as bleach,
isopropyl alcohol and automotive fluids
• Formulated a durable material with abrasion
resistance, UV stability, and tolerant of
temperatures from 0°-140°F
• Delivered surety of supply vs. incumbent material
LubriOne™ PKE Polyketone Formulations
KEY REQUIREMENTS
WHY AVIENT?
https://www.avient.com/sites/default/files/2024-08/Versaflex-Seat Ventilation Tube-Case study Snapshot_0826.pdf
Seat Ventilation Tube Case Study Snapshot
L E A D I N G LU X U RY
C A R M A N U FAC T U R E R
S E A T V E N T I L A T I O N T U B E
• Reliable sealing performance
• Good bonding ASA+PBT
• Excellent chemical resistance and good flexibility
• Provided a TPE with good flexibility to
maintain a tight seal within the ventilation
system, preventing air leaks and ensuring
efficient airflow
• Formulated a durable and chemically
resistant grade to help withstand the various
stresses and environmental conditions that
the ducts may encounter
• Offered quick technical support to fix the
leak problem for customer
Versaflex Thermoplastic Elastomers
KEY REQUIREMENTS
WHY AVIENT?
https://www.avient.com/sites/default/files/2024-03/Aircraft Flooring Case Study Snapshot.pdf
A I RC R A F T I N T E R I O R
O E M
A I R C R A F T F L O O R I N G
• Meet aircraft flammability requirements (FAA)
• Provide flame retardance and smoke mitigation
• Maintain physical properties
• Control viscosity and allow enhanced processability
• Retain product integrity as contaminant free
• Provide product traceability
• Provided strong global EHS and regulatory support
to minimize risk
• Offered a solution to improve quality consistency and
control viscosity
• Enhanced mixing capability and improved
processing temperature and imprint hold
• Allowed greater security of supply with multiple
manufacturing locations
• Provided an integrated solution of plastisols and
pigment dispersions that met traceability
requirements with JIT delivery
KEY REQUIREMENTS
QUALITY + PERFORMANCE
WHY AVIENT?
https://www.avient.com/sites/default/files/308837_en_46388.pdf
C/Carretera.
https://www.avient.com/sites/default/files/2020-07/case-study-one-pager-custom-pa-grade-heat-shield-component.pdf
AUTOMOTIVE OEM
H E A T S H I E L D C O M P O N E N T F O R
L E D H E A D L A M P
• The material needed to solve a hot spot issue
• A PA based grade
• High thermal conductivity - 20 W/mK
• Electrically conductive
• Improved the parts long-term outdoor
performance
• Improved processability compared to high
temperature plastics, reducing tooling costs
• Reduced part weight by 37% than the previous
metal part, providing the customer with a more
economical solution
Customized PA based grade
KEY REQUIREMENTS WHY AVIENT?