https://www.avient.com/resources/safety-data-sheets?page=2934
PG 173289.00 WT PE
ORANGE PE
https://www.avient.com/resources/safety-data-sheets?page=5175
PE TAN LINERS
PE BLUE P285C NO UV
https://www.avient.com/resources/safety-data-sheets?page=1676
PE 152 ORNG 1701-1
PE 152 LT BLU 1698-2
https://www.avient.com/resources/safety-data-sheets?page=45
679-BN-50 BROWN PE CONCENTRATE
886-YE-50 YELLOW PE CONCENTRATE
https://www.avient.com/resources/safety-data-sheets?page=4747
PE TINY TYS BLUE 293C
DARK YELLOW PE V2
https://www.avient.com/news/avient-announces-asia-manufacturing-and-availability-cesa-non-pfas-process-aid
It can be used in polyethylene (PE) and polypropylene (PP) films for flexible packaging, as well as cast PP films and PE tubing for various food packaging applications, such as stand-up pouches, labeling tubes, and laminated tubes.
https://www.avient.com/sites/default/files/2020-10/2020-gravi-tech-design-guide-.pdf
Base Resin ABS PA PBT PC PE PEEK PP PPS
Barrel Temperatures °F (°C)
Rear Zone 400–475(200–250)
480–540
(248–282)
480–520
(250–270)
480–570
(250–300)
400–445
(200–230)
660–700
(350–475)
400–440
(200–225)
520–600
(270–300)
Center Zone 410–480(205–253)
490–550
(254–287)
485–525
(251–273)
500–580
(260–305)
410–455
(207–237)
670–710
(357–385)
410–450
(205–230)
550–610
(285–310)
Front Zone 420–490(210–257)
500–560
(260–293)
490–530
(254–276)
515–590
(267–310)
420–465
(213–243)
680–720
(363–400)
420–455
(215–235)
570–620
(300–320)
Nozzle 425–500(215–260)
510–570
(265–298)
490–540
(254–282)
530–600
(275–315)
430–475
(220–250)
700–730
(370–395)
430–460
(220–240)
610–620
(320–325)
Melt Temperature 425–515(215–270)
510–570
(265–298)
490–540
(254–282)
530–615
(275–325)
430–495
(220–260)
700–725
(370–385)
430–475
(220–250)
610–635
(320–335)
Mold Temperature 140–200(60–90)
150–300
(65–148)
140–280
(60–137)
160–240
(70–115)
80–140
(25–60)
300–400
(150–200)
80–140
(25–60)
190–300
(90–150)
Drying Parameters
190 (90)
2–4 Hours
0 .01%–0 .15%
180 (82)
4–5 Hours
0 .10%–0 .20%
275 (135)
3–4 Hours
0 .02%–0 .04%
250 (125)
3–4 Hours
0 .02%
160 (70)
2 Hours
300 (150)
3–4 Hours
0 .10%
160 (70)
2 Hours
280 (135)
2–3 Hours
0 .01%–0 .20%
Nozzle Type General Purpose Nylon or Reverse Taper General Purpose General Purpose General Purpose General Purpose General Purpose General Purpose
Injection Velocity1 2–5 in/sec; 50–127 mm/sec
Injection Pressure 1,000–2,000 psi; 7–14 Mpa
Back Pressure 50–100 psi; 0 .3–0 .7 Mpa
Screw Speed 25–75 RPM
Cushion 0 .125–0 .250 in; 3–6 mm
Screw Compression Ratio2 2 .0:1–2 .5:1
Comments
1 .
Venting Guidelines by Resin
• PC: .001"–.002" depth & .250" width
• PC/PSU: .002"–.003" depth & .250" width
• PES: .003"–.004" depth & .250" width
• PEI: .001"–.003" depth & .250" width
• PP: .001"–.002" depth & .250" width
• ABS: .0015"–.0025" depth & .250" width
• PEEK: .002"–.004" depth & .250" width
FIGURE 40 - Venting Guidelines
Vent Groove
Vent Land
Vent
FIGURE 44 - Venting guidelines
FIGURE 43 - Venting areas
20 Gravi-Tech
CHAPTER 5 | PROCESS OPTIMIZATION
Process optimization ensures a quality process and
minimizes cycle time.
https://www.avient.com/products/polymer-colorants/fluoropolymer-color-concentrates/colorant-chromatics-pvdf-colorants
PES/PSU/PPSU Colorants: Colorant Chromatics™
https://www.avient.com/products/engineered-polymer-formulations/flame-retardant-formulations/maxxam-sy-foamable-flame-retardant-formulations
With better heat and crush resistance versus foamed PE and FEP, Maxxam SY formulations also include options for 'zero halogen, low smoke and fume.'
https://www.avient.com/products/polymer-colorants/fluoropolymer-color-concentrates/colorant-chromatics-dispersed-pigments-ptfe
PES/PSU/PPSU Colorants: Colorant Chromatics™